Add to Cart
High quality lower price aluminum metal plate 3003 1100 aluminium alloy sheet
Mill finish, this is the most popular of the formable grades of aluminum sheet. It conforms to Federal Specification QQ-A-250/2 and the principal alloying element is manganese, in amounts from 1.0 to 1.5%. It is non-heat treatable and has excellent weldability and corrosion resistance
3003 aluminum plates react well to mechanical finishing and organic finishes. our aluminum sheet has a wide range of sizes readily available to the AMS 4008 for H14
3003 Aluminum Alloy has good machinability and welding is readily accomplished by means of conventional welding methods. Commonly used in chemical equipment, ductwork, and in general sheet metal work. 3003 Aluminum is typically used in stampings and the manufacturing of pressure vessels, builder's hardware, garage doors, awning slats, refrigerator panels, gas lines, gasoline tanks, heat exchangers, drawn and spun parts, and storage tanks. All of our 3003 Aluminum Sheet is protected on one side with a protective vinyl film.
Aluminum sheet metal is great for most custom metal fabrication.
The following are the most commonly used aluminum grades that our customers require.
1104-H14
Commercially pure aluminum, chemical and weather resistant. Ductile, with good weldability, but it is weak. RuiYi customers use it in jewelry and chemical applications.
2024-T3
2024 fabrication typically revolves around aerospace applications. This type of aluminum alloy has great machinability, fair corrosion resistance, is heat treatable and has good workability and appearance.
3003-H14
3003-H14 maintains good weldability and formability, and is corrosion resistant. customers use 3003-H14 in mail boxes, cabinets, tanks, stampings, spun and drawn parts, and fan blades.
5052-H32
5052-H32 has been great for customer use in electronic chassis, tanks, and pressure vessels. While stronger than 3003 it is still formable and has high corrosion resistance and weldability.
6061-T6
6061-T6 is a head treatable structural alloy. customers like the great weldability, corrosion resistance, and great strength.
Chemical Analysis of aluminum alloy Plate | ||||||||||
Alloy | Si | Fe | Cu | Mn | Mg | Cr | Ni | Zn | Ti | Al |
1050 | 0.25 | 0.4 | 0.05 | 0.05 | 0.05 | - | - | 0.05 | 0.03 | Remains |
1060 | 0.25 | 0.35 | 0.05 | 0.03 | - | - | - | - | - | Remains |
1070 | 0.2 | 0.25 | 0.04 | 0.03 | 0.03 | - | - | - | - | Remains |
1100 | 0.95 | 0.95 | 0.05-0.2 | 0.05 | - | - | 0.1 | - | - | Remains |
1200 | 1 | 1 | 0.05 | 0.05 | - | - | - | 0.1 | 0.05 | Remains |
3003 | 0.6 | 0.7 | 0.05-0.2 | 1.0-1.5 | - | - | - | 0.1 | - | Remains |
5005 | 0.3 | 0.7 | 0.2 | 0.2 | 0.5-1.1 | 0.1 | - | 0.25 | - | Remains |
5042 | 0.2 | 0.35 | 0.15 | 0.2--.5 | 3.0-4.0 | 0.1 | - | 0.25 | 0.1 | Remains |
5052 | 0.25 | 0.4 | 0.1 | 0.1 | 2.2-2.8 | 0.15-0.35 | - | 0.1 | - | Remains |
5083 | 0.4 | 0.4 | 0.1 | 0.4-1.0 | 4.0-4.9 | 0.05-0.25 | - | 0.25 | - | Remains |
5754 | 0.4 | 0.4 | 0.1 | 0.5 | 2.6-3.6 | 0.3 | - | 0.2 | - | Remains |
6061 | 0.4-0.8 | 0.7 | 0.15-0.4 | 0.15 | 0.8-1.2 | 0.04-0.35 | - | 0.25 | - | Remains |
6063 | 0.2-0.6 | 0.35 | 0.1 | 0.1 | 0.45 | 0.1 | - | 0.1 | - | Remains |
6082 | 0.7-1.3 | 0.5 | 0.1 | 0.4-1.0 | 0.6-1.2 | 0.25 | - | 0.2 | - | Remains |
7050 | 0.12 | 0.15 | 2.0-2.6 | 0.1 | 1.9-2.6 | 0.04 | - | 5.7-6.7 | 0.06 | Remains |
7075 | 0.4 | 0.5 | 1.2-2.0 | 0.3 | 2.1-2.9 | 0.18-0.28 | - | 5.1-6.1 | 0.2 | Remains |